Home/Products/Non-ionic polyacrylamide
GB/T 17514-2017 · Hydrolysis ≤ 5 mol%

Non-ionic polyacrylamide,
for the pH range where anionic stops working.

[ CH2–CH(CONH2) ]n  ·  Hydrolysis ≤ 5 mol%  ·  MW 4–12 × 10⁶

Below pH 5 the carboxylate groups on an anionic chain protonate, the coil collapses, and bridging stops. Non-ionic PAM keeps its chain extended and its amide groups free to hydrogen-bond — the reason it is specified for acid leach circuits, coal preparation and drilling fluids.

≤5mol% HYDROLYSIS
4–12 MMOLECULAR WEIGHT
pH 2–7WORKING RANGE
24 moSHELF LIFE
CH₂
CH
CONH₂
CH₂
CH
CONH₂
CH₂
CH
CONH₂
CH₂
Non-ionic repeat unit — [CH₂–CH(CONH₂)]n · amide side groups
01 — Grade range

Low charge,
long chain, pH-independent.

With hydrolysis at or below 5 mol% there is almost no carboxylate on the chain, so the molecule behaves the same at pH 2 as at pH 7. The four grades differ mainly in molecular weight, which sets how much shear the solution will tolerate.

HQ-N04
4–6M
Molecular weight
Hydrolysis≤ 3 mol%
Dissolution35–45 min
Best forHigh-shear, dense slurry
Fast-dissolving grade for high-shear circuits and thick slurries where a longer chain would break before it reached the particle.
HQ-N06
6–8M
Molecular weight
Hydrolysis≤ 5 mol%
Dissolution40–50 min
Best forCoal, acid leach
The workhorse for coal preparation and acid leach counter-current decantation.
HQ-N10
10–12M
Molecular weight
Hydrolysis≤ 5 mol%
Dissolution50–65 min
Best forDrilling fluids, low-shear
Higher bridging length for drilling fluids, low-shear thickening and fine-particle retention.
HQ-N08
6–8M · high salt
Molecular weight
Hydrolysis≤ 5 mol%
Salt toleranceHigh
Best forBrine, seawater
Salt-tolerant variant for seawater-based systems and brine-clarification duty.

Hydrolysis values are titration results on the finished powder. A truly zero-hydrolysis homopolymer is available on request for sensitive applications, at 5 t minimum. Viscosity and dissolution figures refer to a 0.1% solution at 25 °C.

02 — Technical data

What the COA will say.

Non-ionic PAM is a narrow product family: the specification is short because the chemistry is. The two figures that matter commercially are hydrolysis and molecular weight.

ParameterSpecificationTest method / note
AppearanceWhite granules or powderVisual
Solid content≥ 90%Drying at 105 °C to constant weight
Degree of hydrolysis≤ 5 mol%Titration; typically 1–3 mol%
Molecular weight4–12 × 10⁶Intrinsic viscosity
Residual acrylamide monomer≤ 0.1%GB/T 17514-2017
Insoluble matter≤ 0.2%Filtration of 0.1% solution
pH of 0.1% solution5–7Glass electrode, 25 °C
Dissolution time35–65 min0.1–0.3% concentration, 25 °C, 60 rpm
Working pH range2–7Performance falls off above pH 8 without a coagulant
Shelf life24 monthsUnopened bag, dry, below 35 °C, out of sunlight
Standard: GB/T 17514-2017. Non-ionic PAM is non-hazardous for transport. TDS, SDS and a sample COA are available before order; SGS or CCIC inspection can be arranged per shipment.
03 — Mechanism

No charge to work with —
so it uses hydrogen bonds instead.

Anionic and cationic polymers adsorb electrostatically. Non-ionic PAM has nothing to attract it to a charged surface, so it relies on amide groups forming hydrogen bonds with surface hydroxyls. Weak individually, strong in aggregate — and unaffected by pH.

STEP 01

Amide groups find the surface

The CONH₂ side groups hydrogen-bond to silanol, oxide and hydroxide surfaces. This works in acid, where anionic carboxylate groups would already be protonated and the chain collapsed into a coil.

STEP 02

Salt does not screen it out

High ionic strength compresses the double layer that anionic and cationic polymers depend on. Hydrogen bonding does not care about ionic strength, so non-ionic grades keep working in brine, seawater and acidic process water.

STEP 03

Bridge with a neutral backbone

With no internal charge repulsion the chain stays extended and can bridge several particles. The trade-off is dose: without electrostatic attraction you need more polymer to cover the same surface, typically 1.5–2× the anionic figure.

04 — Applications and dose ranges

Where non-ionic PAM earns its cost.

Dose figures are product per unit of feed, adjusted upward from textbook values to reflect plant practice. Non-ionic duty generally runs at a higher dose than anionic for the same solids load.

Acid leach & CCD circuits

Gold, copper and uranium acid leach counter-current decantation, pH 1.5–3. Clarifies overflow and improves underflow density without pH adjustment.

30–120 g/t solids · grades N06 / N10

Coal preparation

Slurry clarification and fine coal recovery in acidic wash water; also tailings thickening where the circuit runs below pH 5.

20–60 g/t solids · grades N04 / N06

Drilling fluids & mud

Viscosifier and fluid-loss control in water-based mud, including brine and seawater systems. Tolerates high calcium and chloride.

1–5 kg/m³ mud · grade N10

Metal finishing & pickling

Acid pickle liquor neutralisation sludge, anodising and plating waste where the liquor is still acidic when the polymer is added.

15–60 g/t solids · grades N04 / N06

Paper & board

Neutral and acid sizing systems, and broke clarification. Used where anionic PAM would be screened out by alum or high salt.

0.3–1.2 kg/t paper · grades N06 / N08

Foundry & refractory wastewater

Dust scrubber water and refractory slurry with high hardness and fine solids that respond poorly to charged polymers.

10–40 g/t solids · grade N04

Not on the list? Non-ionic PAM also runs in sugar beet and cane juice clarification, in textile sizing recovery, and in soil conditioning. If your water is under pH 5 or above 3% salt, tell us — that single fact usually decides between non-ionic and anionic.

05 — Preparation and dosing

Slow to wet out,
slow to hydrate, worth the wait.

Non-ionic powder is the slowest of the three families to dissolve. Under-hydrated solution is the most common reason a plant concludes “non-ionic doesn't work”.

Make-down procedure

01Dilute to 0.1–0.3% w/w. Use warm process water (30–40 °C) where available — it cuts hydration time by a third.
02Disperse at 500–800 rpm. Non-ionic granules wet out slowly and float. A eductor or powder-water disperser pays for itself here.
03Hydrate at ~60 rpm for 45–65 min. Do not shorten this. Undissolved granules behave like inert fines and blind filters.
04Use within 24 hours. Non-ionic solutions are biologically vulnerable — a warm tank grows bacteria overnight.
05Check the pH at the injection point. Above pH 8 the amide groups begin to hydrolyse in solution, which slowly turns the product anionic and changes its behaviour mid-shift.

Five things that quietly ruin performance

Under-hydration. Non-ionic grades need the full 45–65 minutes. A solution with visible gel particles is not a solution.

Cold water. Below 15 °C hydration time doubles; in winter, dose from a warmed make-down tank or extend the residence time.

Alkaline process water. Above pH 8 the product starts to hydrolyse in the tank. Make down in the least alkaline water available.

Assuming it replaces anionic 1:1. Without electrostatic attraction the dose is typically 1.5–2× the anionic figure for the same solids. Budget for it.

Shear before the floc forms. Long chains are the whole point; a centrifugal transfer pump after the injection point removes the benefit.

06 — Packaging and logistics

Loaded to the port you name.

25 kg woven bag

PE-lined PP woven bag with inner liner, 40 bags per pallet or 40 loose bags per bundle.

20–25 t per 20' FCL

750 kg jumbo bag

Four-loop FIBC with discharge spout, for plants with bulk hoppers and no manual handling.

18–20 t per 20' FCL

Terms and documents

FOB Shanghai / Qingdao, CIF, or DDP where we have a forwarder. COA, SDS, packing list and certificate of origin included.

Non-hazardous cargo · no DG declaration
07 — Compliance

What we hold, and
what we do not.

Non-ionic PAM carries the same national standard as the anionic family, with the same limits on residual monomer.

✓

GB/T 17514-2017

Produced and tested to the Chinese national standard for water-treatment polyacrylamide.

✓

ISO 9001 / 14001

Quality and environmental management certified across the production sites.

✓

SGS / CCIC

Third-party inspection available per shipment, at buyer's request and cost.

✕

No NSF/ANSI 60

We do not hold it. For US municipal drinking-water duty requiring that certification, we decline the enquiry.

On the drinking-water question. A low-monomer non-ionic grade at ≤ 0.025% residual acrylamide can be produced for potable-water duty, but it is a separate run and still carries no NSF/ANSI 60 mark. If your specification names NSF, this is the wrong product family.

08 — Questions buyers actually ask

Before you specify non-ionic.

When is non-ionic better than anionic?

Two conditions: pH below 5, or high ionic strength. In acid, anionic carboxylate groups protonate and the chain coils; in brine, the double layer collapses and electrostatic adsorption weakens. Non-ionic PAM relies on hydrogen bonding, which neither condition affects.

Does it really work at pH 2?

Yes — that is the point of it. Activity is essentially flat from pH 2 to 7. Above pH 8 the amide groups start to hydrolyse in solution, which slowly converts the product to an anionic behaviour and cuts its shelf life in the tank to hours rather than a day.

Why is the dose higher than anionic?

Because there is no electrostatic attraction pulling the chain onto the particle. Coverage depends on random collision and hydrogen bonding, so more polymer is needed. Budget 1.5–2× the anionic figure for the same solids load, and let a jar test confirm it.

Can it be used in seawater or brine?

Yes, and it is the right choice there. The N08 variant is produced for high-chloride and high-calcium systems; anionic PAM in the same water loses a significant part of its viscosity and its bridging performance.

What is the MOQ and lead time?

1 ton for a trial, 20–25 t per 20' container. Stock grades ship within 7–10 days of order confirmation; a custom hydrolysis or molecular weight runs 20–25 days.

How is it stored?

Dry, sealed, on pallets, below 35 °C, out of sunlight — 24 months. Once made down, use the solution within 24 hours and keep the tank covered; non-ionic solutions support bacterial growth in warm weather.

Next step

Acid, brine or both?
That decides the grade.

Send the pH, ionic strength, solids load and the equipment the polymer will feed. We reply with a grade, a dose range and a sample dispatch date.

Reply within 12 working hours · data used for quotation only